The number of atomic layers of graphene and the sensing area of graphene significantly impact the responsivity and response/recovery time of graphene-based humidity sensors on SiO2/Si substrate.
บทคัดย่อ
The researchers fabricated humidity sensors on SiO2/Si substrate using monolayer, double-layer, and tri-layer graphene. They studied the impact of the number of atomic layers of graphene and the sensing area of graphene on the responsivity and response/recovery time of the prepared humidity sensors.
Key highlights:
- The responsivity of graphene-based humidity sensors decreased with the increase in the number of atomic layers of graphene under the same sensing area conditions. Monolayer graphene-based devices showed the highest responsivity, while tri-layer graphene-based devices showed the lowest.
- The sensing area of graphene also affected the responsivity, with larger sensing areas (75 μm × 72 μm) exhibiting higher responsivity compared to smaller sensing areas (45 μm × 72 μm) under the same number of atomic layers.
- Regarding response and recovery time, monolayer graphene-based devices showed the fastest response and recovery, while double-layer graphene-based devices showed the slowest. Tri-layer graphene-based devices exhibited the fastest overall response and recovery time.
- The researchers chose double-layer graphene-based devices, which had relatively good responsivity and stability, for applications in human respiration monitoring and contact-free finger monitoring.
สถิติ
The relative resistance change of monolayer graphene-based devices is over 5 times larger than that of tri-layer graphene-based devices under the same sensing area of 75 μm × 72 μm.
The response time of monolayer graphene-based devices is around 6.66-8.64 seconds, while the recovery time is around 9.45-12.59 seconds.
The response time of double-layer graphene-based devices is around 12.26-17.21 seconds, and the recovery time is around 21.23-34.06 seconds.
The response time of tri-layer graphene-based devices is around 4.96-5.09 seconds, and the recovery time is around 8.67-9.89 seconds.
คำพูด
"The relative resistance change of graphene-based devices decreased with the increase of number of atomic layers of graphene under the same change of relative humidity."
"Devices based on tri-layer graphene showed the fastest response/recovery time while devices based on double-layer graphene showed the slowest response/recovery time."